| Al-Mg-La体系富Al区液相限的研究 |
| 郑朝贵;邢娅;钱久信;叶于浦 |
| 北京大学化学系;北京大学化学系;北京大学化学系;北京大学化学系 |
|
| AN INVESTIGATION ON LIQUIDUS OF Al-RICH CORNER OF Al-Mg-La SYSTEM |
| ZHENG Chaogui; XING Ya; QIAN Jiuxin; YE Yupu (Department of Chemistry; peking University) |
引用本文:
郑朝贵;邢娅;钱久信;叶于浦. Al-Mg-La体系富Al区液相限的研究[J]. 金属学报, 1983, 19(6): 61-66.
,
,
,
.
AN INVESTIGATION ON LIQUIDUS OF Al-RICH CORNER OF Al-Mg-La SYSTEM[J]. Acta Metall Sin, 1983, 19(6): 61-66.