| 硼钢淬透性与硼向奥氏体晶界的偏聚 |
| 贺信莱;褚幼义;柯俊 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| THE HARDENABILITY OF BORON STEEL AND THE SEGREGATION OF BORON |
| HE Xinlai; CHU Youyi; KE Jun (T. Ko) (Beijing University of Iron and Steel Technology) |
引用本文:
贺信莱;褚幼义;柯俊. 硼钢淬透性与硼向奥氏体晶界的偏聚[J]. 金属学报, 1983, 19(6): 5-114.
,
,
.
THE HARDENABILITY OF BORON STEEL AND THE SEGREGATION OF BORON[J]. Acta Metall Sin, 1983, 19(6): 5-114.
1 Grange, R.A.; Shortsleeve, F.J.; Hilty, D.C.; Binder, W.O.; Motock, G. T.; Offenhauer, C.M., Boron, Calcium, Calumbium and Zirconium in Iron and Steel, Wiley, New York, 1957, p. 1-57. 2 Brownrigy, A., J. Aust. Inst. Met., 18 (1973) , 124. 3 Kapadia, B.N., Hardenablity Concepts with Application to Steer, Proc. of a Symp. Held at the Sheraton-Chicago Hotel, Oct. 1977, Eds. Dovne, D. V.; Kirkaldy, J.S., Metall. Soc. AIME, 1978, p.448. 4 Morral, J.E.; Cameron, T.B., Boron in Steel, Proc. of the Int. Symp. on Boron Steel, Milwaukee, Wisconsin, Sept. 1979, Eds. Banerji, S.K.; Morral, J.E., Metall. Soc. AIME, 1980, p.19. 5 Simcoe, C.R.; Elsea, A.R.; Manning, G.K., Trans. AIME, 203 (1955) , 193. 6 Melloy, G.F.; Slimmon, P.R.; Podyursky, P.P., Metall. Trans., 4 (1973) , 2279. 7 土生隆一;宫田政祐;関野昌藏;合田进,铁鋼,60(1974) ,1470. 8 Williams, T.M.; Stoneham. A.M.; Harries, D.R., Met Sci., 10 (1976) , 14. 9 贺信莱;褚幼义;张秀林;余宗森;李秋萍;尹熙光,金属学报,13 (1977) ,2. 10 Keown, S.K.; Pickering, F.B., Met. Sci., 11 (1977) , 225. 11 Ueno, M.; Lnonc, T., Trans. Iron Steel Inst. Jpn., 13 (1973) , 210. 12 #12 13 贺信莱;褚幼义;柯俊,金属学报,18 (1982) ,1. 14 贺信莱;褚幼义;柯俊,ibid.,18 (1982) ,11. 15 贺信莱;褚幼义;柯俊,中美双边冶金学术会议论文集,1981,p.532. (英文版). 16 褚幼义;贺信莱;余宗森;欧宇光,金属学报,16 (1980) ,386. 17 Maitrepierre, Ph.; Thivellier, D.; Rofesvernis, J.; Rousseau, D.; Tricot, R., Hardenability Concepts with Application to Steel, Proc. of a Symp. held at the Sheraton-Chicago Hotel, Oct. 1977, Eds. Dovne, D.V.; Kirkaldy, J.S., Metall. Soc. AIME, 1978, p.421. 18 贺信莱;褚幼义,理化检验(物理分册),(1975) ,№5,29;№6,25. 19 He, X.L. (贺信莱); Chu, Y.Y. (褚幼义), J. Phys. D: Appl. Phys., 16 (1983) , 1145-1158. 20 沈鹏,金属学报,11(1975) ,33. 21 Maittrepierre, Ph.; Thivellier, D.; Tricot, R., Mem. Sci. Rev. Metall., 70 (1973) , 893. 22 Mclean, D., Grain Boundaries in Metals, Oxford, 1957, p.116 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|