| Astroloy合金弯曲晶界对蠕变断裂特性的影响 |
| 郭桂雄;蔡其巩;申辉旺 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| EFFECT OF WAVY GRAIN BOUNDARY ON CREEP FRACTURE BEHAVIOUR IN ASTROLOY ALLOY |
| GUO Guixiong; CAI Qigong; SHEN Huiwang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
郭桂雄;蔡其巩;申辉旺. Astroloy合金弯曲晶界对蠕变断裂特性的影响[J]. 金属学报, 1983, 19(6): 13-23.
,
,
.
EFFECT OF WAVY GRAIN BOUNDARY ON CREEP FRACTURE BEHAVIOUR IN ASTROLOY ALLOY[J]. Acta Metall Sin, 1983, 19(6): 13-23.
1 Larson, J.M.; Floreen, S., Metall. Trans., 8A (1977) , 51. 2 Merrick, H.H.; Floreen, S., Metall. Trans., 9A (1978) , 231. 3 Landes, J.D.; Begley, J.A., Am. Soc. Test. Mater., Spec. Tech. Publ., 590, (1976) , 128. 4 Nikbin, K.M.; Webster, G.A.; Turner, C.E., Am. Soc. Test. Mater., Spec. Tech. Publ., 601, (1976) , 47. 5 Goldman, N.L.; Hutchinson, J. W., Int. J. Solids Struct., 11 (1975) , 575. 6 Shih, C.F.; Hutchinson, J.W., J. Eng. Mater. Technol., 98 (1976) , 289. 7 蔡其巩,金属学报,12 (1976) ,45. 8 蔡其巩,ibid., 13 (1977) ,246. 9 Kumar, V.; German, M.D.; Shih, C.F., EPRI-Report, NP-1931, Palo Alto, (1980) . 10 Kubo, S.; Ohji, K.; Ogura, K., Eng. Pract. Mech., 11 (1979) , 315. 11 Miyagawa, O.; Yamamoto, M.; Kobayshi, M., Superalloys: Metallurgy and Manufacture, Eds. Kear, B.H. et al, Claitor's Publ., Baton Rouge, Louisiana, 1976, p.245. 12 Raj, R.; Ashby, M.F., Metall. Trans., 2 (1971) , 1113. 13 Gifkins, R.C., ibid., 7A (1976) , 1225. 14 Eberhardt, A.; Baudelet, B., Philos. Mag., 41 (1980) , 843. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|