| 圆盘形夹杂的断裂力学参数 |
| 蒋生蕊;张宏图 |
| 兰州大学;兰州大学 |
|
| A NOTE ON FRACTURE MECHANICS PARAMETERS OF DISK INCLUSIONS |
| JIANG Shengrui; ZHANG Hongtu (Lanzhou University) |
引用本文:
蒋生蕊;张宏图. 圆盘形夹杂的断裂力学参数[J]. 金属学报, 1983, 19(5): 69-80.
,
.
A NOTE ON FRACTURE MECHANICS PARAMETERS OF DISK INCLUSIONS[J]. Acta Metall Sin, 1983, 19(5): 69-80.
1 Bilby, B.A.; Eshelby, J.D., Fracture, Vol.1: Microscopic and Macroscopic Fundamentals, Ed. Liebowitz, H., Academic Press, 1968, p.99. 2 张宏图,折晓黎,物理学报,30(1981) ,761. 3 折晓黎,张宏图,ibid.,32 (1983) ,182. 4 徐祖耀,马氏体相变和马氏体,科学出版社,1980,p.103. 5 Esheby, J.D., Proc. R. Soc., A241 (1957) , 376. 6 Esheby, J. D., ibid., A252 (1959) , 561. 7 Esheby, J.D., Progress in Solid Mechanics, Vol. Ⅱ, Eds. Snedden, I.N., Hill, R., North-Holland, 1961, p.87. 8 村外志夫;森勉,転位介在物,培风馆,1976,p.23. 9 Kroener, E., Z. Phys., 151. (1958) , 504. 10 Macmillan, W. D., The Theory of the Potential, Dover Publ., New York, 1958, p.62. 11 北京钢铁研究院金属物理室,工程断裂力学,上册,国防工业出版社,1977,p.53,54. 12 Tada, H.; Paris P.C.; Irwin, G., The Stress Analysis of Cracks Handbook, Hellerlown, Pennsylvania, 1973, p.24. 1, 24. 7. 13 Esheby, J.D., Solid State Physics, Vol.3, Eds. Seilz, F.; Turnbull, D., Academic Press, New York, 1956, p.79. 14 Hull, D., Acta Metall., 9 (1961) , 191.y |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|