| 近零磁伸金属玻璃饱和磁伸常数的退火和温度依赖性 |
| 陈笃行 |
| 冶金工业部钢铁研究总院 |
|
| ANNEALING AND TEMPERATURE DEPENDENCE OF MAGNETOSTRICTION IN NEARLY ZERO-MAGNETOSTRICTIVE METALLIC GLASSES |
| CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
陈笃行. 近零磁伸金属玻璃饱和磁伸常数的退火和温度依赖性[J]. 金属学报, 1983, 19(5): 58-64.
.
ANNEALING AND TEMPERATURE DEPENDENCE OF MAGNETOSTRICTION IN NEARLY ZERO-MAGNETOSTRICTIVE METALLIC GLASSES[J]. Acta Metall Sin, 1983, 19(5): 58-64.
1 Sherwood, R.C.; Gyorgy, E. M.; Chen, H.S.; Ferris, S.D.; Norman, G,; Leamy, H.J., AIP Conf. Proc., (1975) , № 24. , 745. 2 Kikuchi, M.; Fujimori, H.; Obi, Y.; Masumoto, T., Jpn. J. Appl. Phys., 14 (1975) , 1077. 3 Gyorgy, E. M.; Leamy, H. J.; Sherwood, R. C.; Chen, H.S., AIP Conf. Proc., (1976) , №29, 198. 4 O'Handley, R.C.; Mendelsohn, L.I.; Nesbitt, E.A., IEEE Trans. Magn., MAG-12 (1976) , 942. 5 Kohmoto, O.; Yamaguchi, N.; Ohya, K.; Fujishima, H.; Ojima, T., IEEE Trans. Magn., MAG-14 (1978) , 949. 6 Kohmoto, O.; Ohya, K.; Yamaguchi, N.; Fujishima, H.; Ojima, T., J. Appl. Phys., 50 (1979) , 5054. 7 Ohnuma, S.; Masumoto, T., J. Appl. Phys., 50(1979) , 7597. 8 Hilzinger, H.R.; Hillmann, H.; Mager, A,, Phys. Status Solidi, A55 (1979) , 763. 9 Hilzinger, H. R.; Kunz, W., J. Magn. Magn. Mater., 15-18 (1980) , Part Ⅲ, 1357. 10 陈笃行,加张力测量非晶软磁带样λ_s的冲击法,待发表. 11 O'Handley, R.C., Phys. Rev., B18 (1978) , 930. 12 O'Handley, R.C.; Sullivan, M.O.,J. Appl. Phys., 52 (1981) , 1841. 13 Egami, T., Mater. Res. Bull., 13 (1978) , 557. 14 Egami, T., J. Mater. Sci., 13 (1978) , 2587. 15 Bozorth, R.M., Ferromagnetism, D.Van Nostrand-Co, New York, 1956, p.664. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|