| 47121β-Ti合金中相变的透射电镜观察 |
| 俞学节 |
| 上海钢铁研究所 |
|
| TEM OBSERVATION OF PHASE TRANSFORMATION IN 47121 β-Ti ALLOY |
| YU Xuejie (Shanghai Institute of Iron and Steel Research) |
引用本文:
俞学节. 47121β-Ti合金中相变的透射电镜观察[J]. 金属学报, 1983, 19(5): 27-152.
.
TEM OBSERVATION OF PHASE TRANSFORMATION IN 47121 β-Ti ALLOY[J]. Acta Metall Sin, 1983, 19(5): 27-152.
1 Williams, J.C., Titanium Science and Technology, Proc. of the Int. Conf. on Titanium, 2nd, Massachusetts Institute of Technology Combridge, Mass., 1972, Eds. Jaffee, R.I.; Burte, H. M., Plenum, New York, 1973, p.1433. 2 Rhodes, C. G.; Williams, J.C., Metall. Trans., 6A (1975) , 2103. 3 Rhodes, C.G., Paton, N. E., ibid., 8A (1977) , 1749. 4 Headley, T.J.; Rack, H.J., ibid., 10A (1979) , 909. 5 Duerig, T,W.; Terlinde, G.T.; Williams, J.C., ibid., 11A (1980) , 1987. 6 Banerjee, D., ibid., 13A (1982) , 681. 7 Feeney, J. A.; Blackburn, M. J., ibid, 1 (1970) , 3309. 8 Fontaine, D. De.; Paton, N.E.; Williams, J. C., Acta Metall., 19 (1971) , 1153. 9 Jon, M. C.; Fujimura, H.; De Angelis, R.J., Metallography, 5 (1972) , 139. 10 Crane, R. L.; Chattoraj, S.C., J. Less-Common Met., 25 (1971) , 225. 11 Blackburn, M. J.; Williams, J.C., Trans. Metall. Soc. AIME, 242 (1968) , 2461. 12 Hickman, B. S., J. Inst. Met., 96 (1968) , 330. 13 Ganesan, P.; Sargent, G.A.; De Angelis, R. J., J. Mater. Sci., 15 (1980) , 1425. 14 Ageyev, N.N.; Petrova, L.V.; Grankova, L.P., Titanium Science and Technology, Proc. of the Int. Conf. on Titanium, 2nd, Massachusetts Institute of Technology, Combridge, Mass., 1972, Eds. Jaffee, R.I.; Burte, H.M., Plenum, New York, 1973, p.1295. 15 Cook, H.E., Acta Metall., 22 (1974) , 239. 16 Hickman, B. S., J. Mater. Sci., 4 (1969) , 554. 17 Williams, J.C.; Hickman, B.S.; Leslie, D.H., Metall. Trans., 2 (1971) , 477. 18 Margolin, Harold; Levine, E.; Young, M., ibid., 8A (1977) , 373. 19 Rhodes, C.G.; Williams, J.C., ibid., 6A (1975) , 1570. 20 Rhodes, C.G.; Paton, N.E., ibid., 10A (1979) , 209. 21 Banerjee, D.; Arunachalam, V.S., Acta Metall., 29 (1981) , 1685.D |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|