| Mg对镍基高温合金蠕变性能的影响 |
| 可大年;仲增墉 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| EFFECT OF Mg CONTENT ON CREEP BEHAVIOUR OF Ni-BASE WROUGHT SUPERALLOY |
| KE Da'nian; ZHONG Zengyong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
可大年;仲增墉. Mg对镍基高温合金蠕变性能的影响[J]. 金属学报, 1983, 19(5): 13-20.
,
.
EFFECT OF Mg CONTENT ON CREEP BEHAVIOUR OF Ni-BASE WROUGHT SUPERALLOY[J]. Acta Metall Sin, 1983, 19(5): 13-20.
1 (1978) , №11 1047. 2 (1979) , №7, 545. 3 (1978) , №11, 59. 4 (1973) , №4, 193. 5 可大年;仲增墉,冶金部钢铁研究总院学报,待发表. 6 Furillo, F. T.; Davidson J. M.; Tien, J. K., Mater. Sci. Eng., 39 (1979) , 267. 7 Ashby, M. F.; Raj, R., Conference on the Mechanics and Physics of Fracture, Organised by The Institute of Physics and the Metals Society, London, 1975, p.1/1-16/11. |
|