| 粒子强化高温合金的滞弹性松弛、循环蠕变和应力断裂行为 |
| 庄毅 |
| 冶金部钢铁研究总院 |
|
| ANELASTIC RELAXATION, CYCLIC CREEP AND STRESS RUPTURE OF PARTICLE STRENGTHENED SUPERALLOYS |
| by ZHUANG Yi (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 14 April; 1982) |
引用本文:
庄毅. 粒子强化高温合金的滞弹性松弛、循环蠕变和应力断裂行为[J]. 金属学报, 1983, 19(4): 26-38.
.
ANELASTIC RELAXATION, CYCLIC CREEP AND STRESS RUPTURE OF PARTICLE STRENGTHENED SUPERALLOYS[J]. Acta Metall Sin, 1983, 19(4): 26-38.
1 Matejczyk, D. E.; Zhuang, Y. (庄毅); Tien, J. K., J. Met. 32 (1980) , №. 8, 24. 2 Matejczyk, D. E.; Zhuang, Y. (庄毅); Tien, J. K., ibid., 32 (1980) , №. 12, 4. 3 Tien, J. K.; Matejczyk, D. E.; Zhuang, Y. (庄毅); Howson, T. E., Creep and Fracture of Engineering Materials and Structures, Proc. of the Int. Conf. Held at University College, Swansea, Eds. Wilshire, B.; Qwen, D. R. J., Prineridge Press, Swansea, U. K., 1981, p. 433. 4 Matejczyk, D. E.; Zhuang, Y. (庄毅); Tien, J. K., Metall. Trans., 14A(1983) , 241. 5 Zhuang, Y. (庄毅); Matejczyk, D. E.; Tien, J. K., to be published. 6 Shetty, D. K.; Meshii, M., Metall. Trans., 6A (1975) , 349. 7 Bradley, W. L.; Nam, S. W.; Matlock, D. K., ibid., 7A (1976) , 425. 8 Coutinho, C. B.; Matlock, D. K.; Bradley, W. L., Mater. Sci. Eng., 21 (1975) , 239. 9 Morris, D. G.; Harries, D. R., J. Mater. Sci., 13 (1978) , 985. 10 Koterazawa, R., Mechanical Behavior of Materials, Vol. 3, The Society of Materials Science, Japan, 1972, p. 135. 11 Rosen, A.; Weiss, L; Baruch, J.; Tzelinik, E., Metall. Trans., 6A (1975) , 1311. 12 Lupinc, V.; Gabrielli, F., Mater. Sci. Eng., 37 (1979) , 143. 13 Morris, D. G., J. Mater. Sci., 13 (1978) , 1849. 14 Gibbons, T. B.; Lupinc, V.; McLean, D., Mater. Sci., 9 (1975) , 437. 15 Howson, T. E.; Stulga, J. E.; Tien, J. K., Metall, Trans., 11A (1980) , 1599. 16 Howson, T. E., Unpublished Research, 1979. 17 Yen, C. T., Unpublished Research, 1981. 18 Orgen, F. E.; Gell, M., Metall. Trans., 2 (1971) , 943. 19 Gell, M.; Leverant, G. R., Mechanisms of High Temperature Fatigue, ASTM STP 520, 1973, p. 37. 20 Lubahn, J. D., Trans. ASM, 45 (1953) , 787. 21 Evans, W. J.; Harrison, G. F., Scr. Metall., 9 (1975) , 239. 22 Gittus, J. H., ibid., 6 (1972) , 247. 23 Gittus, J. H., ibid., 6 (1972) , 481. 24 Meshii, M.; Ueki, M.; Chiou, H. D., Strength of Metals and Alloys, Vol. 1, Proc. of the 5th Int. Conf., Aachen, W. Germany, Aug. 1979, Eds. Haasen, P; Gerold, V.; Kostorz, G., Pergamon Press, New York, 1979, p. 245. 25 Parker, J. D.; Wilshire, B., Philos. Mag., 41 (1980) , 665.A |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|