| Cu-Al-Zn-Mn-Ni合金的马氏体形态和形状记忆效应 |
| 赵连城;孙东立;雷廷权 |
| 哈尔滨工业大学;哈尔滨工业大学;哈尔滨工业大学 |
|
| MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Zn-Mn-Ni ALLOY |
| by ZHAO Liancheng; SUN Dungli; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 22 June; 1982; revised manuscript 20 November; 1982) |
引用本文:
赵连城;孙东立;雷廷权. Cu-Al-Zn-Mn-Ni合金的马氏体形态和形状记忆效应[J]. 金属学报, 1983, 19(4): 19-144.
,
,
.
MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Zn-Mn-Ni ALLOY[J]. Acta Metall Sin, 1983, 19(4): 19-144.
1 Buehler, W. J; Gilfrich, J. V., J. Appl. Phys., 34 (1963) , 1475. 2 赵连城;郭松;雷廷权;金属学报,17(1981) ,506. 3 Saburi, T.; Wayman, C, M., Acta Metall., 28 (1980) , 15. 4 高村仁一,金属物理,5(1959) ,135. 5 汪复兴,金属物理,机械工业出版社,1981,p.88. 6 赵连城;戴虹;雷廷权,金属热处理学报,3(1982) ,36,2 |
|