| 裂纹顶端位错的运动和小范围屈服的K_(Ⅱc) |
| 龙期威;高桦 |
| 中国科学院金属研究所;中国科学院力学研究所 |
|
| THE DISLOCATION MOTION AT CRACK TIP AND K_(Ⅱc) OF SMALL SCALE YIELDING MATERIALS |
| by LONG Qiwei (LUNG Chi-wei) (Institute of Metal Research; Academia Sinica; Shenyang); GAO Hua (Institute of Mechanics; Academia Sinica; Beijing) |
引用本文:
龙期威;高桦. 裂纹顶端位错的运动和小范围屈服的K_(Ⅱc)[J]. 金属学报, 1983, 19(3): 65-71.
,
.
THE DISLOCATION MOTION AT CRACK TIP AND K_(Ⅱc) OF SMALL SCALE YIELDING MATERIALS[J]. Acta Metall Sin, 1983, 19(3): 65-71.
1 Erdogan, F.; Sih, G. C., J. Basic Eng., 85 (1963) , 519. 2 Sih, G. C., Methods of Analysis and Solutions of Crack Problems, Nordhoff Int. Publ., Leyden, 1973, p. 221. 3 Wang Tzuchiang (王自强), Advance in Research on the Strength and Fracture of Materials, Vol. 4, 4th Int. Conf. Fracture, June 1977, Canada, Eds. Taplin, D. M. R., p.135. 4 高桦;王自强;杨成寿;周爱华,金属学报,15(1979) ,380. 5 Bilby, B. A.; Swinden, K. H., Proc. R. Soc., (London), Ser. A285 (1965) ,22. 6 Vitek, V., J. Mech. Phys., Solids, 24 (1976) , 263. 7 Riedel, H., ibid., 24 (1976) , 277. 8 D.布洛克,工程断裂力学基础,王克仁等译,科学出版社,1980,p.276. 9 Lung Chi-wei(龙期威),Scientia Sinica(中国科学),23(1980) .441. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|