| 3Cr3Mo3VNb钢贝氏体回火时的相及组织转变 |
| 冯干江;沈凤歧;陈铭谟 |
| 西北工业大学;西北工业大学;西北工业大学 |
|
| PHASE AND STRUCTURE TRANSFORMATION OF BAINITE IN 3Cr3Mo3VNb STEEL DURING TEMPERING |
| FENG Ganjiang; SHEN Fengqi; CHEN Mingmo (North-Westen Polytechnical University; Xi'an) |
引用本文:
冯干江;沈凤歧;陈铭谟. 3Cr3Mo3VNb钢贝氏体回火时的相及组织转变[J]. 金属学报, 1983, 19(2): 23-148.
,
,
.
PHASE AND STRUCTURE TRANSFORMATION OF BAINITE IN 3Cr3Mo3VNb STEEL DURING TEMPERING[J]. Acta Metall Sin, 1983, 19(2): 23-148.
1 Jatczk, C. F., ASM Trans. Q., 58(1965) , 195. 2 Simcoe, C. R.; Nehrenbery, A. E., ASM Trans. Q., 58(1965) , 378. 3 Tunney, R. J.; Ridley, N., Met. Sci., 13(1979) , 585. 4 Tunney, R. J.; Lorimer, G. W.; Ridley, N., Met. Sci., 12(1978) , 271. 5 Inoue, A.; Masumoto, T., Metall. Trans., 11A(1980) , 739. 6 Raynor, D.; Whiteman, J. A.; Honeycombe, R. W. K,, J. Iron Steel Inst., 204(1966) , 349. 7 Hopkin, L. M. T.; Jenkinson, E. A., J. Iron Steel Inst., 202(1964) , 929. 8 西田卓彦;谷野满,日本金属学会志,29(1965) ,728. 9 Smith, R.; Iron Steel Inst. Spec. Rep., №64(1959) , 307. 10 Nutting, J., J. Iron Steer Inst., 207(1969) , 872. 11 Hippsley, C. A., Met. Sci., 15(1981) , 137. 12 Seal, A. K.; Honeycombe, R. W. K., J. Iron Steel Inst., 188(1958) , 343. 13 Ridal, K. A.; Quarrell, A. G., J. Iron Steel Inst., 200(1962) , 359. 14 Lupton, J. B.; Murphy, S.; Woodhead, J. H., Metall. Trans., 3A(1972) , 2923. 15 Schulz, B. J.; McMahon, C. J., Jr., Metall. Trans., 4A(1973) , 2485. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|