| 计算机模拟二元系结晶过程的分凝现象 |
| 胡兹莆;姚连增 |
| 中国科学技术大学;中国科学技术大学 |
|
| COMPUTER SIMULATION OF SEGREGATION IN BINARY SYSTEM CRYSTALLIZATION |
| HU Zipu; YAO Lianzeng (University of Science and Technology of China; Hefei) |
引用本文:
胡兹莆;姚连增. 计算机模拟二元系结晶过程的分凝现象[J]. 金属学报, 1983, 19(1): 109-114.
,
.
COMPUTER SIMULATION OF SEGREGATION IN BINARY SYSTEM CRYSTALLIZATION[J]. Acta Metall Sin, 1983, 19(1): 109-114.
1 Gilmer, G. H., J. Cryst. Growth, 42(1977) , 3. 2 Gilmer, G. H.; Jackson, K. A., 1976 Crystal Growth and Materials, eccg-1 Zurich, Eds. Kaldis, E.; Scheel, H. J., North-Holland, Amsterdam, 1977, p. 79. 3 Muller-Krumbhaar, H., Monte-Carlo Methods in Statistical Physics, Ed. Binder, K., Sprinser-Verlag, Berlin, 1979, p. 290. 4 Gilmer, G. H.; Bennema, P., J. Cryst. Growth, 13/14(1972) , 148. 5 Leamy, H. J.; Gilmer, G. H.; Jackson, K. A., Surface Physics of Materials, Ed. Blakely, J. M., Academic Press, New York, 1975, p. 121. 6 郑兆勃;胡兹莆,物理,10(1981) ,368._ |
|