| 若干简单金属与类金属在Ag中固溶度亚稳扩展的研究 |
| 周新铭;靳嘉禄;宁远涛;赵钟民 |
| 冶金工业部贵金属研究所;冶金工业部贵金属研究所;冶金工业部贵金属研究所;冶金工业部贵金属研究所 |
|
| METASTABLE EXTENSION OF SOLID SOLUBILITY OF CERTAIN SIMPLE METALS OR METALLOIDS IN Ag |
| Zhou Xinming; Jin Jialu; Ning Yuantao; Zhao Zhongmin (Institute of Precious Metals Research; Kunming) |
引用本文:
周新铭;靳嘉禄;宁远涛;赵钟民. 若干简单金属与类金属在Ag中固溶度亚稳扩展的研究[J]. 金属学报, 1982, 18(5): 534-539.
,
,
,
.
METASTABLE EXTENSION OF SOLID SOLUBILITY OF CERTAIN SIMPLE METALS OR METALLOIDS IN Ag[J]. Acta Metall Sin, 1982, 18(5): 534-539.
1 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 1-57. 2 Elliot, R. P., Constitution of Binary Alloys, First Supplement, McGraw-Hill, New York, 1965, 1-22. 3 Pearson, W. B., A Handbook of Lattice Spacings and Structure of Metals and Alloys, Pergamon Press, London, 1958, p. 259-308. 4 Anantharaman, T. R.; Romachandrarao, P.; Suryanarayana, C.; Lele, S.; Chattopadnyay, K., Trans. Indian Inst. Met., 30 (1977) , 425. 5 Duwez, P., ASM Trans Q., 60 (1967) , 607. 6 Anantharaman, T. R.; Suryanarayana, C., J. Mater. Sci., 6 (1971) , 1111. 7 Klement, W., Jr.; Luo, M. L., Trans Metall. Soc. AIME, 227 (1963) , 1253. 8 Miedema, A. R.; Boom, R.; de Boor, F. R., J. Less-Common Met., 41 (1975) , 283. 9 Miedema, A. R., ibid., 46 (1976) , 67. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|