| 30MnNiMoCu铸钢无光泽小棱面断口的研究 |
| 毛晓禹;欧宇光;李芝;徐全新;李玉海 |
| 内蒙古金属材料研究所;内蒙第一机械厂;内蒙第一机械厂;内蒙第一机械厂;内蒙第一机械厂 |
|
| AN INVESTIGATION OF DARK FACET FRACTURE IN CAST STEEL 30MnNiMoCu |
| Mao Xiaoyu (Nei Monggol Institute of Materials Research; Baotou) Ou Yuguang Li Zhi Xu Quanxin Li Yuhai (Nei Monggol № 1 Machine Works) (Manuscript received 26 May; 1980; revised; manuscript 5 August; 1981) |
引用本文:
毛晓禹;欧宇光;李芝;徐全新;李玉海. 30MnNiMoCu铸钢无光泽小棱面断口的研究[J]. 金属学报, 1982, 18(4): 418-522.
,
,
,
,
.
AN INVESTIGATION OF DARK FACET FRACTURE IN CAST STEEL 30MnNiMoCu[J]. Acta Metall Sin, 1982, 18(4): 418-522.