| 硼向奥氏体晶界的非平衡偏聚 |
| 贺信莱;褚幼义;柯俊 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| THE NON-EQUILIBRIUM SEGREGATION OF BORON TO AUSTENITE GRAIN BOUNDARIES |
| He Xinlai; Chu Youyi; Ke Jun (T. Ko) (Beijing University of Iron and Steel Technology; Beijing) |
引用本文:
贺信莱;褚幼义;柯俊. 硼向奥氏体晶界的非平衡偏聚[J]. 金属学报, 1982, 18(1): 1-10.
,
,
.
THE NON-EQUILIBRIUM SEGREGATION OF BORON TO AUSTENITE GRAIN BOUNDARIES[J]. Acta Metall Sin, 1982, 18(1): 1-10.
1 Simcoe, C. R.; Elsea, A. R.; Manning, G. K., Trans. AIME, 203 (1955) , 193. 2 Simcoe, C. R.; Elaea, A. R.; Manning, G. K., ibid., 206 (1956) , 984. 3 Goldhoff, R. M.; Spretnak, J. W., ibid., 209 (1957) , 1278. 4 McLean, D., Grain, Boundaries in Metals, Clarendon Press, Oxford, 1957, p,. 116-150. 5 Jandeska, W. F.; Morral, J. E., Metall. Traits., 3 (1972) , 2933. 6 Adair, A. M.; Spretnak, J. W.; Speiser, R., Trans. AIME, 203 (1955) , 353. 7 Mortal, J. E.; Cameron, T. B., Metall. Trans., 8 (1977) , 1817. 8 Sharma, R. C.; Purdy, G. R., ibid., 4(1973) , 2303. 9 Ueno, M.; Lnoue, T., Trans. Iron Steel Inst. Jpn., 13 (1973) , 210. 10 Gladman, T., BSC, Swinden 实验室未发表工作,转引自:LIewellyn, D. T.; Cook, W. T., Met. Technol. 1 (1974) , 517. 11 Keown, S. R., Scand. J. Metall., 2 (1973) , 59. 12 Williams, T. M.; Stoneham, A. M.; Harries, D. R., Met. Sci., 10 (1976) , 14. 13 Keown, S. R.; Pickering, F. B., ibid., 11 (1977) , 225. 14 贺信莱,褚幼义,张秀林,余宗森,李秋萍,尹熙光,金属学报,13(1977) ,2. 15 贺信莱,褚幼义,余宗森,欧宇光,金属学报,16(1980) ,386. 16 沈鹏,金属学报,11(1975) ,33. 17 Mattrepierre, P.; Thivellier, D.; Tricot, R., Mere. Sci. Rev. Metall., 70 (197) , 893. 18 Armijo. J. S.; Rosenbaum. H. S., J. Appl. Phys., 38 (1967) , 2064. 19 贺信莱,褚幼义,柯俊,金属学报,18(1982) ,11. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|