金属学报  1981, Vol. 17 Issue (5): 609-627    
  论文 本期目录 | 过刊浏览 |
中国金属学会第二届全国金相图片展览获奖作品选登
No Author
AWARDED PHOTOS SELECTED FROM THE SECOND METALLOGRAPHIC EXHIBITION
No Author
引用本文:

No Author. 中国金属学会第二届全国金相图片展览获奖作品选登[J]. 金属学报, 1981, 17(5): 609-627.
. AWARDED PHOTOS SELECTED FROM THE SECOND METALLOGRAPHIC EXHIBITION[J]. Acta Metall Sin, 1981, 17(5): 609-627.

全文: PDF(12808 KB)  
摘要: 中国金属学会于1980年举办了第二届全国金相图片展览。有十八个省、市、自治区的九十个单位,选送来光学金相图片和电子金相图片共二千余张,经过初评,选出813张公开展览。其中光学显微照片包括:铸铁与碳钢、合金钢、不锈钢、高温合金、有色金属、钢中夹杂、焊缝组织及其它;电子显微照片包括:电子显微镜复型、金属薄膜和扫描电子显微镜拍摄的照片。此外,尚有彩色金相照片、特殊金相方法照片和金相艺术照片。 1980年10月,金属学及金属物理学术会议开会期间,举行首展。经到会人员投票选举,评选委员会审议,学术委员会复审,决定73幅为获奖图片。计有光学金相图片一等奖5幅,二等奖16幅,三等奖28幅;电子金相照片二等奖2幅,三等奖22幅。 本刊将这些图片按先光学金相照片后电子金相照片的顺序刊出,个别分图较多的图片做了适当节选。全部图片均注明试样处理经过,浸蚀剂和观察所得,以供参考。
Abstract:The Second Metallographic Exhibition sponsored by The Chinese Society of Metals was held first in Shenyang on October 1980 and going to tour through the country. More than two thousand optical and electron photomicrographs were the preliminary choice from ninety institutes and laboratories of eighteen provinces, municipalities and autonomous regions. 813 photos were selected in the Exhibition opened to the public. The optical micrographs of them include cast iron and carbon steel, alloy, stainless steel, superalloy, non-ferrous metals, inclusions in steel, weld structure, etc.; the electron micrographs were taken by replica, metallic foil or SEM. Some colour micrographs and ones Shot by special techniques or with aesthetic microstructure are also displayed.The Judging Panel gave awards to 73 photos, they are:Optical microscopy Electron microscopy 1st award 5 2nd award 16 2 3rd award 28 22 These awarded photos will be published in two issues of the Acta Metal. lurgica Sinica, Vol. 17(1981), No. 5 and 6.The title, winner name and affiliation are classified in a list. And also a brief record of the treatment of specimen, etchant used and remark on observation is made for each photo.