| RECo_5热膨胀反常研究 |
| 杨应昌;何文望;林勤 |
| 北京大学;北京大学;北京大学 |
|
| THERMAL EXPANSION ANOMALIES OF THE COMPOUNDS RECo_5 |
| Yang Yingchang; Ho Wenwang and Lin Qin (Belling University) |
引用本文:
杨应昌;何文望;林勤. RECo_5热膨胀反常研究[J]. 金属学报, 1981, 17(1): 67-72.
,
,
.
THERMAL EXPANSION ANOMALIES OF THE COMPOUNDS RECo_5[J]. Acta Metall Sin, 1981, 17(1): 67-72.
[1] Jennings, L. D. and Chipman, D. R., Amer. Inst. Phys. Conf. Proc., № 18, 1973, p. 1187. [2] Buschow, K. H. J,, Miedema, A. R. and Brouha, M., J. Less-Common Metals, 38 (1974) , 9. [3] 孙天铎、祝景汉、王德文,金属学报,15(1979) ,58. [4] Neel, L., Ann. Phys.,5(1936) , 232. [5] Yang,Y.T.(杨应昌),Ho,W.W.(何文望),Yang,L.K.(杨继廉)Tchou,T.S.(朱家瑄), Tseng,S.S.(曾祥欣)et Kin,L.(金兰),J.Phys.,Colloq. C5, Supplement au N°5,Tome 40,Mai 1979,p.C5-117. |
|