| 高钛低铝高温合金电渣重熔中钛烧损的研究 |
| 陈崇禧;王涌;傅杰;陈恩普 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| A STUDY ON THE TITANIUM LOSS DURING ELECTROSLAG REMELTING HIGH TITANIUM AND LOW ALUMINUM CONTENT SUPERALLOY |
| Chen Chongxi; Wang Yong; Fu Jie and Chen Enpu (Beijing University of Iron and Steel Technology) |
引用本文:
陈崇禧;王涌;傅杰;陈恩普. 高钛低铝高温合金电渣重熔中钛烧损的研究[J]. 金属学报, 1981, 17(1): 50-57.
,
,
,
.
A STUDY ON THE TITANIUM LOSS DURING ELECTROSLAG REMELTING HIGH TITANIUM AND LOW ALUMINUM CONTENT SUPERALLOY[J]. Acta Metall Sin, 1981, 17(1): 50-57.
[1] Elienne, M. and Mitchell, A., Oxidation Losses of Low Levels of Titanium During Electroslag Remelting,Second International Symposium on Electroslag Remelting Technology Proceedings Part Ⅱ,Pittsburgh,Mellon Institute,1969, ed. by G. K. Bhat. [2] Knights, C. F. and Perkins, R., Electroslag Refining, London, 1973, Iron and Steel Institute, p.35. [3] Gill, L. L. and Harris, K., Electroslag Refining, London, 1973, Iron and Steel Institute, p.89. |
|