| 应力腐蚀开裂过程中的表面形变 |
| 张百伟;杜家驹 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| SURFACE DEFORMATION IN THE COURSE OF STRESS CORROSION CRACKING |
| Zhang Baiwei and Du Jiaju (Institute of Metal Research; Academia Sinica) |
引用本文:
张百伟;杜家驹. 应力腐蚀开裂过程中的表面形变[J]. 金属学报, 1981, 17(1): 18-120.
,
.
SURFACE DEFORMATION IN THE COURSE OF STRESS CORROSION CRACKING[J]. Acta Metall Sin, 1981, 17(1): 18-120.
|