| 电炉高铝砖炉顶渣蚀层的显微镜观察 |
| 高振昕 |
| 冶金工业部洛阳耐火材料研究所 |
|
| MICROSCOPIC STUDY ON SLAGGED HIGH-ALUMINA ARC FURNACE ROOF BRICKS |
| Gao Zhenxin Luoyang Institute of Refractory Research |
引用本文:
高振昕. 电炉高铝砖炉顶渣蚀层的显微镜观察[J]. 金属学报, 1980, 16(4): 480-504.
.
MICROSCOPIC STUDY ON SLAGGED HIGH-ALUMINA ARC FURNACE ROOF BRICKS[J]. Acta Metall Sin, 1980, 16(4): 480-504.
[1] Greaves, E. I. and Lakin, J. R., Trans. Brit. Cer. Soc., 70 (1971) , 39. [2] Weidmuller, C. and Suckow, A., Tonind-Ztg. Keram. Rundsch., 98 (1974) , Nr. 7, 159. [3] Spencer, D. R. F, May, J. and Ball, N., Trans. Brit. Cer. Soc., 72(1973) , 125.W |
|