| 稀土元素对Fe-Cr-Al合金氧化皮结合力的影响 |
| 章复中;孙传岳 |
| 包头冶金研究所;上海电工合金厂 |
|
| EFFECTS OF RARE EARTH ADDITIONS ON THE COHESION OF OXIDE SCALE IN AN Fe-Cr-Al ALLOY |
| Zhang Fuzhong;Sun Chuanyue Baotou Institute of Metallurgy Research and Shanghai Electrical Alloy Plant |
引用本文:
章复中;孙传岳. 稀土元素对Fe-Cr-Al合金氧化皮结合力的影响[J]. 金属学报, 1980, 16(4): 394-400.
,
.
EFFECTS OF RARE EARTH ADDITIONS ON THE COHESION OF OXIDE SCALE IN AN Fe-Cr-Al ALLOY[J]. Acta Metall Sin, 1980, 16(4): 394-400.
[1] Wukusick, C. S., Mater. Res. Stand., 4 (1964) , 637. [2] Golightly, F. A., Stott, F. H. and Wood, G. C., Oxid. Metals, 10 (1976) , 163. [3] Tien, J. K. and Pettit, F. S., Met. Trans., 3 (1972) , 1587. [4] 骆继勋,银耀德,林生昆,赵齐,王俭,金属学报,13(1977) ,263. [5] Jan, J. P., Steinemann, S. and Dinichert, P., J. Phys. Chem. Solids, 12 (1960) , 349. [6] Warshaw, S. I. and Norton, F. H., J. Amer. Cer. Soc., 45 (1962) , 479. [7] Cahoon, H. P. and Chrislensen, C. J., J. Amer. Cer. Soc. 39 (1956) , 337.s |
|