| 天然气直接渗碳的热重法研究 |
| 谭志诚;周立幸;谭辉玲;梅文麟 |
| 中国科学院大连化学物理研究所;中国科学院大连化学物理研究所;重庆大学冶金系;重庆大学冶金系 |
|
| THERMOGRAVIMETRIC STUDY OF DIRECT CARBURIZING BY NATURAL GAS |
| Tan Zhicheng;Zhou Lixing;Tan Huiling;Mei Wenlin Dalian Institute of Chemical Physics; Academia Sinica Dept. of Metallurgy; Chongqing University |
引用本文:
谭志诚;周立幸;谭辉玲;梅文麟. 天然气直接渗碳的热重法研究[J]. 金属学报, 1980, 16(2): 239-244.
,
,
,
.
THERMOGRAVIMETRIC STUDY OF DIRECT CARBURIZING BY NATURAL GAS[J]. Acta Metall Sin, 1980, 16(2): 239-244.
|