| 铝合金中位错与替代式溶质原子交互作用引起的低频振幅内耗峰 |
| 葛庭燧 |
| 中国科学院金属研究所 |
|
| LOW-FREQUENCY "AMPLITUDE PEAKS" IN THE INTERNAL FRICTION ASSOCIATED WITH THE INTERACTION OF SUBSTITUTIONAL SOLUTE ATOMS WITH DISLOCA-TIONS IN ALUMINIUM ALLOYS |
| Ge Tingsui (T. S. Kê) Institute of Metal Research; Academia Sinica |
引用本文:
葛庭燧. 铝合金中位错与替代式溶质原子交互作用引起的低频振幅内耗峰[J]. 金属学报, 1980, 16(2): 218-230.
.
LOW-FREQUENCY "AMPLITUDE PEAKS" IN THE INTERNAL FRICTION ASSOCIATED WITH THE INTERACTION OF SUBSTITUTIONAL SOLUTE ATOMS WITH DISLOCA-TIONS IN ALUMINIUM ALLOYS[J]. Acta Metall Sin, 1980, 16(2): 218-230.
[1] Ke,T.S.(葛庭燧),Phys.Rev.,76(1949) ,470. [2] Ke,T.S.(葛庭燧),Trans.AIME,188(1950) ,575. [3] Ke,T.S.(葛庭燧),Phys.Rev.,78(1950) ,420. [4] Ke,T.S.(葛庭燧),Science Record(科学记录),3(1950) ,61. [5] 葛庭燧,张进修,物理学报,21(1965) ,1711. [6] 葛庭燧,张进修,物理学报,22(1966) ,71. [7] 葛庭燧,张志舜,张进修,物理学报,22(1966) ,270. [8] 潘正良,王中光,孔庆虎,葛庭燧,待发表. [9] Seeger, A. and Schiller, P., Act. Met., 10 (1962) , 348. [10] Couch, W. E. and Swartz, J. E., Phil. Mag., 7 (1962) , 1231. [11] Perez, J., Peguin, P. and Gobin, P., Rev. Phys. Appl. 4 (1969) , 437. [12] Stadelmann, P. and Benoit, W., Internal Friction and Ultrasonic Attenuation in Solids, Ed. R. R. Hasiguti and N. Mikoshiba, University of Tokyo Press, 1977, p. 573, Fig. 2. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|