| 液态La_2O_3-CaF_2和La_2O_3-CaF_2-CaO-SiO_2渣中La_2O_3的活度 |
| 王常珍;邹元爔 |
| 东北工学院;中国科学院上海冶金研究所 |
|
| ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS |
| Wang Changzhen;Zou Yuanxi (Chou Yuan-hsi) North-Eastern Polytechnical Institute Shanghai Institute of Metallurgy; Academia Sinica |
引用本文:
王常珍;邹元爔. 液态La_2O_3-CaF_2和La_2O_3-CaF_2-CaO-SiO_2渣中La_2O_3的活度[J]. 金属学报, 1980, 16(2): 190-194.
,
.
ACTIVITY OF La_2O_3 IN LIQUID La_2O_3-CaF_2 AND La_2O_3-CaF_2-CaO-SiO_2 SLAGS[J]. Acta Metall Sin, 1980, 16(2): 190-194.
[1] 王渭源,邹元爔,金属学报,6(1963) ,40. [2] 邹元爔,赵彭年,曹兆民,金属学报,6(1963) ,121. [3] Chou Yuan-hsi (邹元爔), Chow Ji-Cheng (周继程), Chao Peng-nian (赵彭年), Sci. Sinica, 12(1963) , 1249. [4] Chou Yuan-hsi (邹元爔), Chao Peng-nian (赵彭年), Sci. Sinica, 11 (1962) , 1287. [5] #12 |
|