| 脱碳工艺对晶粒取向3%Si-Fe磁性的影响 |
| 罗阳;张百成;周秀媛;马鸿良 |
|
| THE EFFECT OF DECARBURIZING PROCESS ON THE MAGNETIC PROPERTIES OF THE GRAIN ORIENTED 3%Si-Fe |
| Luo Yang;Zhang Baicheng;Zhou Xiuyuan;Ma Hongliang |
引用本文:
罗阳;张百成;周秀媛;马鸿良. 脱碳工艺对晶粒取向3%Si-Fe磁性的影响[J]. 金属学报, 1980, 16(1): 38-130.
,
,
,
.
THE EFFECT OF DECARBURIZING PROCESS ON THE MAGNETIC PROPERTIES OF THE GRAIN ORIENTED 3%Si-Fe[J]. Acta Metall Sin, 1980, 16(1): 38-130.
[1] 钢铁研究院硅钢研究组,金属学报,13(1977) ,80. [2] #12 [3] 中国科学院数学研究所统计组,常用数理统计方法,科学出版社,1973年. [4] Beck, P.A. Kremer, J.C., Demer, L.J. and Holzworth, M.L. Trans. AIME, 175 (1948) , 372. [5] Coble, R.C., J. Appl. Phys., 32 (1961) , 793. [6] Hu, H. and Rath, B. B. Met. Trans., 1 (1970) , 3181 |
|