| 昆钢赤铁矿球团固结过程中Fe_2O_3的板状生长和交连现象 |
| 刘富有 |
| 昆钢中心试验室 |
|
| THE GROWTH AND CROSS-CONNEXION OF Fe_2O_3 PLATELETS IN CONSOLIDATION OF HEMATITE PELLET |
| Liu Fuyou Central Laboratory of Kunming Iron and Steel Company |
引用本文:
刘富有. 昆钢赤铁矿球团固结过程中Fe_2O_3的板状生长和交连现象[J]. 金属学报, 1980, 16(1): 18-126.
.
THE GROWTH AND CROSS-CONNEXION OF Fe_2O_3 PLATELETS IN CONSOLIDATION OF HEMATITE PELLET[J]. Acta Metall Sin, 1980, 16(1): 18-126.
|