| 稀土对两种锰磷低合金钢回火脆化的影响 |
| 戢景文;肖连芳;高怀荪 |
| 包头冶金研究所;包头冶金研究所;包头冶金研究所 |
|
| THE EFFECT OF RARE EARTH MISCHMETAL ON THE TEMPER BRITTLENESS OF TWO LOW ALLOY STEELS CONTAINING MANGANESE AND PHOSPHORUS |
| Ji Jingwen;Xiao Lianfang;Gao Huaisun Baotou Institute of Metallurgy |
引用本文:
戢景文;肖连芳;高怀荪. 稀土对两种锰磷低合金钢回火脆化的影响[J]. 金属学报, 1980, 16(1): 115-138.
,
,
.
THE EFFECT OF RARE EARTH MISCHMETAL ON THE TEMPER BRITTLENESS OF TWO LOW ALLOY STEELS CONTAINING MANGANESE AND PHOSPHORUS[J]. Acta Metall Sin, 1980, 16(1): 115-138.
[1] Viswanathan, R.. Met. Trans., 2 (1971) , 809. [2] 陈篪,姚蘅,邓枝生,庄韬,邓其源,科学通报,20(1975) ,329.A |
|