| 一种快速注释电子通道花样的方法 |
| 蓝芬兰;廖乾初 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| A RAPID METHOD FOR INDEXING THE ELECTRON CHANNELLING PATTERN |
| Lan Fenlan;Liao Qianchu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry |
引用本文:
蓝芬兰;廖乾初. 一种快速注释电子通道花样的方法[J]. 金属学报, 1980, 16(1): 104-108.
,
.
A RAPID METHOD FOR INDEXING THE ELECTRON CHANNELLING PATTERN[J]. Acta Metall Sin, 1980, 16(1): 104-108.
[1] Van Essen, C.G., Schulson, E.M. and Danaghay, R.H., Nature, 225 (1970) , 847; J. Met. Sci., 6 (1971) . 213. [2] Schulson, D.E., J. Sci. Inst., 2 (1969) , 361; J. Appl. Phys., 42 (1971) , 3894. [3] Newburg, D.E. and Jop. D.C., Proc. 25th Anniversary Meeting of EMAG., Cambridge, 1971, p. 306. [4] 廖乾初,王云,王鸿君,物理学报,28(1979) ,279 |
|