| Y_2(Fe_(1-x)Ni_x)_(17)的磁性及其穆斯保尔谱线的研究 |
| 杨应昌 |
| 北京大学物理系 |
|
| THE MAGNETIC PROPERTIES AND MOSSBAUER SPECTRA OF Y_2(Fe_(1-x)Ni_x)_(17) |
| Yang Ying-chang( Dept. of Physics; Beijing University) |
引用本文:
杨应昌. Y_2(Fe_(1-x)Ni_x)_(17)的磁性及其穆斯保尔谱线的研究[J]. 金属学报, 1978, 14(1): 51-57.
.
THE MAGNETIC PROPERTIES AND MOSSBAUER SPECTRA OF Y_2(Fe_(1-x)Ni_x)_(17)[J]. Acta Metall Sin, 1978, 14(1): 51-57.
[1] Barbara, B. et al., Int. J. Magn., 4 (1973) , 77. [2] Givord, D. and Lemaire, R., IEEE Trans. Magn., Mag-10 (1974) , 109. [3] Narashimhan, K. S. V. L. and Wallace, W. E., AIP Conf. Proc., 18 (1973) , 1248. [4] Gubbens, P. C. M. et al., J. Phys. (Paris), Collq., C6, 35 (1974) , suppl, au No. 12, C6-617. [5] Gubbens, P. C. M. and Buschow, K. H. J., J. Appl. Phys., 44 (1973) , 3739. |
|