| 单边裂纹梁横向力弯曲下的应力强度因子 |
| 潘灏 |
|
| THE STRESS INTESITY FACTORS OF A SINGLEEDGE CRACKED BAR LOADED BY IN-PLANE TRANSVERSE FORCES |
| Pan Hao |
引用本文:
潘灏. 单边裂纹梁横向力弯曲下的应力强度因子[J]. 金属学报, 1977, 13(4): 301-307.
.
THE STRESS INTESITY FACTORS OF A SINGLEEDGE CRACKED BAR LOADED BY IN-PLANE TRANSVERSE FORCES[J]. Acta Metall Sin, 1977, 13(4): 301-307.
[1] 陈篪,力学,(1974) ,№ 3,121. [2] Brown, W. F. Jr. and Srawley, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ., No. 410, (1966) . [3] Srawley, J. E. and Gross, B., Eng. Fract. Mech., 4 (1972) , 587. [4] Wilson, W. K., Eng. Fract. Mech., 2 (1970) , 169. [5] Benthem, J. P. and Koiter, W. J., Mechanics of Fracture, vol. Ⅰ, ed. by G. C. Sih, Noordhoff International Publishing, Leyden, the Netherlands, (1973) , 131. [6] Tada, H., Paris, P. C. and Irwin, G. R., The Stress Analysis of Crack Handbook, Del Research Corp., Hellertown, Pa., U. S. A., 1973.- |
|