| 关于J积分和应变能间的关系式 |
| No Author |
| 金属研究所断裂研究组 |
|
| No Author |
引用本文:
No Author. 关于J积分和应变能间的关系式[J]. 金属学报, 1976, 12(2): 162-171.
.
[J]. Acta Metall Sin, 1976, 12(2): 162-171.
[1] Rice, J.R. et al., Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 536, 1973, p. 231. [2] 陈篪等,科学通报,7(1975) ,329. [3] 金属研究所待发表工作. [4] Green, A. P. and Hundy, B. B., Quart. J. Mech. Appl. Math., 6(1953) , 223. [5] Brown, W. F. and Srawley, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ. No.410, 1967,13. [6] Benthem, J. P. and Koiter, W. T., Mechanics of Fracture, ed. by Sih, G.C., 1973, Vol. 1, 131. [7] Kies, J. A. et al.,Amer. Soc. Test. Mater., Spec. Tech. Publ. No. 381, 1965, 328. [8] 陈篪,金属学报,12(1976) ,129. |
|