| 某些镍基高温合金蠕变性能的研究 |
| 陈篪;邓枝生 |
|
| No Author |
引用本文:
陈篪;邓枝生. 某些镍基高温合金蠕变性能的研究[J]. 金属学报, 1975, 11(1): 59-111.
,
.
[J]. Acta Metall Sin, 1975, 11(1): 59-111.
[1] Monkman, F.C. and Grant, N.J., Deformation and Fracture at Elevated Temperatures, ed. by N.J. Grant and A.W. Mullendore, MIT, 1965, pp. 91-103. [2] 陈箎等,物理学报,23 0974) ,69. [3] Johnson, W.R. et al., Met. Trans., 3 (1972) , 963. [4] Lange, W., Phys. Status Solidi, 5 (1964) , 63. [5] Heslop, J., J. Inst. Metals, 91 (1962-63) , Part 1, 28. [6] Conrad, H. et al., Joint International Conference on Creep, Session Ⅰ, Paper 20, publ. by Inst. Mech. Eng., London, 1963. [7] Leverant, G.R. and Kent, B.H., Met. Trans., 1 (1970) , 491. [8] Chaudhuri, A., J. Inst. Metals, 98 (1970) , 114. [9] Mukherjee, A.K. et al., ASM Trans. Quart., 62 (1969) , 155. [10] Garofalo, F., Fundamentals of Creep and Creep-Rupture in Metals, Macmillan, 1965. [11] Weertman, J., J. Appl. Phys., 28 (1957) , 1185. [12] Flinn, P.A., Trans. AIME, 218 (1960) , 145. [13] Barrett, C.R. and Nix, W.D., Acta Met., 13 (1965) , 1247. [14] Wolf, H., Z. Naturforsch., 15A (1960) , 180. [15] 陈篪等,金属学报,8(1965) ,232. [16] Webster, G.A. and Piearcey, B.J., Metal Sci. J., 1 (1967) , 97. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|