| 液相烧结RCo_5永磁体中矫顽力的分布 |
| 孙天铎;臧树义;冯劲愚 |
|
| No Author |
引用本文:
孙天铎;臧树义;冯劲愚. 液相烧结RCo_5永磁体中矫顽力的分布[J]. 金属学报, 1975, 11(1): 42-50.
,
,
.
[J]. Acta Metall Sin, 1975, 11(1): 42-50.
[1] Becker, J.J., J. Appl. Phys., 42 (1971) , 1537. [2] Zijlstra, H., J. Appl. Phys., 42 (1971) , 1510. [3] Schweizer, J. et al., IEEE Trans. Magn., 7 (1971) , 429. [4] Inomata, K. et al., Jap. J. Appl. Phys., 12 (1973) , 565. [5] Westendorp, F.F., Solid State Commun., 8 (1970) , №3, 139. [6] Den Broeder, F.J.A. and Buschow, K.H.J., J. Less-Common Metals, 29 (1912) , 65. [7] Buschow, K.H.J., J. Less-Common Metals, 29 (1972) , 283. [8] #12 [9] McCurrie, R.A., Phil. Mag., 22 (1970) , 1013. [10] McCurrie, R.A. and Gaunt, P., Phil. Mag., 13 (1966) , 567. [11] Gaunt, P., J. Appl. Phys., 43 (1972) , 637. |
|