| 含氟化氫高炉煤气对三号結构鋼的高溫腐蝕 |
| 金大康;沈邦儒;黄永书 |
| 中国科学院冶金研究所;中国科学院冶金研究所;中国科学院冶金研究所 |
|
| HIGH TEMPERATURE CORROSION OF MILD STEEL IN BLAST FURNACE EXHAUST GAS CONTAINING HF |
| CHIN TA-K'ANG; SHN PANG-JU; HUANG YUNG-SHU; (Institute oF Metallurgy; Academia Sinica) |
引用本文:
金大康;沈邦儒;黄永书. 含氟化氫高炉煤气对三号結构鋼的高溫腐蝕[J]. 金属学报, 1966, 9(1): 90-97.
,
,
.
HIGH TEMPERATURE CORROSION OF MILD STEEL IN BLAST FURNACE EXHAUST GAS CONTAINING HF[J]. Acta Metall Sin, 1966, 9(1): 90-97.
[1] #12 [2] Myers, W. R., DeLong, W. B.: Chem. Eng. Progr., 1948, 44, 559. [3] Hignett, T. P., Siegel, M. R.: Ind. Eng. Chem., 1949, 41, 2493. [4] Wartenberg, H. V., Bosse, O.: Z. Elektrochem., 1922, 28, 384. [5] Froning, J. F., Richards, M. K., Stricklin, T. W. et al.: Ind. Eng. Chem., 1947, 39, 275. [6] Lenfesty, F. A., Farr, T. D., Brosheer, J. C.: Ind. Eng. Chem., 1952, 44, 1448. [7] Simons, J. H.: Fluorine Chemistry, (Academic, 1950) , vol. 1, p. 248. [8] Kellogg, H. H.: Trans. AIME, 1951, 191, 137. [9] Kubaschewski, O., Evans, E. LL.: Metallurgical Thermochemistry, 2nd ed., (Pergamon, 1956) , p. 333. [10] Jellinek, K., Rudat, A.: Z. Anorg. Allgem. Chem., 1928, 175, 281. [11] Wrazei, W. J.: J. Iron Steel Inst. (London), 1944, 149, 227. [12] Peiser, H. S., Rooksby, H. P., Wilson, A. J. C.: X-Ray Diffraction by Polycrystalline Materials, (Inst. Phys., London, 1955) , p. 503. [13] Mellor, J. W.: A Comprehensive Treatise on Inorganic and Theoretical Chemistry, (Longmans, Green and Company, 1935) , vol. 14, p. 1. [14] Quill, L. L.: The. Chemistry and Metallurgy of Miscellaneous Materials, Thermodynamics, (McGraw-Hill, 1950) , p. 202.C |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|