| α鈦中的应变时效 |
| 王其闵;章熙康 |
|
| STRAIN AGEING OF α-TITANIUM |
| WANG CH'I-MIN; CHANG HSI-K'ANG |
引用本文:
王其闵;章熙康. α鈦中的应变时效[J]. 金属学报, 1965, 8(4): 484-490.
,
.
STRAIN AGEING OF α-TITANIUM[J]. Acta Metall Sin, 1965, 8(4): 484-490.
[1] Nabarro, F. R. N.:Report of a Conference on Strength of Solids, (Phys. Soc., London, 1948) , p.38. [2] Cottrell, A. H.:Report of a Conference on Strength of Solids, (Phys. Soc., London, 1948) , p. 30. [3] Cottrell, A. H., Bilby, B. A.:Proc. Phys, Soc., 1949, A62, 49. [4] Harper, S.:Phys. Rev., 1951, 83, 709. [5] Boiling, G. F.:Phil. Mag., 1959, 4, 537. [6] Russell, B.:Phil. Mag., 1963, 8, 615. [7] Russell, B., Vela, P.:Phil. Mag., 1963, 8, 677. [8] Wintenberger, M.:Compt. Rend., 1957, 244, 2800. [9] Coulomb, P., Friedel, J.:Dislocations and Mechanical Properties of Crystals, (Wiley, 1957) , p. 558. [10] Rosi, F. D., Perkins, F. C.:Trans. Am. Soc. Metals, 1953, 45, 972. [11] Holden, F. C., Ogden, H. R., Jaffee, R. I.:Trans. AIME, 1953, 197, 238. [12] Portevin, A., Le Chatelier, F.:Acad. Sci. (Paris), 1923, 176, 507. [13] McReynolds, A. W.:Trans. AIME, 1949, 185, 32. [14] Phillips, V. A., Swain, A. J., Eborall, R.:J. Inst. Metals, 1953, 81, 625. [15] Wilcox, B. A,. Smith, G. C.:Ada Met., 1964, 12, 371. [16] Manjeine, M. J.:Trans. ASME, 1944, 66, A-211. [17] Cottrell, A. H.:Phil. Mag., 1953, 44, 829. [18] Cottrell, A. H.:Dislocations and Plastic Flow in Crystals, (Oxford Univ. Press, 1953) , p. 139. [19] Gupta, D., Weinig, S.:Trans. AIME, 1959, 215, 209. [20] Wasilewski, R. J.:Trans. Am. Soc. Metals, 1963, 56, 221. [21] Seitz, F.:Advan. Phys., 1952, 1, 43. [22] Mott, N. F.:Phil. Mag., 1952, 43, 1151. [23] Mott, N. F.:Phil. Mag., 1953, 44, 187, 742. [24] #12 [25] #12 [26] 吳自良、王其闵:物理学报,1958,14,354. Wu Tzu-liang(吳自良),Wang Chi-mia(王其闵):Sci.Sinica,1958,7,1029. [27] Poe, W. P., Palmer, H. R., Opie, W. R.:Trans. Am. Soc. Metals, 1960, 52, 191. [28] Gupta, D., Weinig, S.:Acta Met., 1962, 10. 292.@ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|