| 鉻-錳-氮奥氏体耐热鋼的时效脆性 |
| 郭蕴宜 |
|
| THE AGING EMBRITTLEMENT OF Cr-Mn-N AUSTENITIC HEAT-RESISTING STEELS |
| KUO YN-YI |
引用本文:
郭蕴宜. 鉻-錳-氮奥氏体耐热鋼的时效脆性[J]. 金属学报, 1965, 8(4): 467-550.
.
THE AGING EMBRITTLEMENT OF Cr-Mn-N AUSTENITIC HEAT-RESISTING STEELS[J]. Acta Metall Sin, 1965, 8(4): 467-550.
[1] 肖纪美:金属学报,1958,3,138. [2] 李有柯、谢仰华、郭蕴宜等:待发表. [3] 郭蕴宜、刘嘉乐、李有柯等:金属学报,1964,7,409. [4] Pennington, W. J.:Metal Progr., 1958, 73, (3) , 82. [5] Brown, J. T.:Metal Progr., 1958, 74, (8) , 87. [6] Decker, R. F., Freeman, J. W.:Trans. AIME, 1960, 218, 277. [7] Bushy, P. E., Warga, M. E., Wells, C:Trans. AIME, 1953, 197, 1463. [8] Koh, P. K.(郭本坚):Trans. AIMB, 1953, 197, 339. [9] 庄育智、刘嘉乐:金属学报,1960,5,24. [10] Clark, C. C., Mihalisin, J. R., Carroll, K. G.:Trans. AIME, 1957, 209, 1210. [11] Cina, B.:J. Iron Steel Inst. (London), 1955, 179, 230. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|