| 间歇式真空感应炉中坩埚供氧的一个来源 |
| 邵象华;知水;赵仁川;曲培迅 |
|
| OXYGEN CONTAMINATION FROM THE CRUCIBLE IN BATCH-TYPE VACUUM INDUCTION MELTING |
| SHAO HSIANG-HUA;CHIH SHUI;CHAO JEN-CHUAN;CHU PEI-HSUN |
引用本文:
邵象华;知水;赵仁川;曲培迅. 间歇式真空感应炉中坩埚供氧的一个来源[J]. 金属学报, 1965, 8(3): 392-394.
,
,
,
.
OXYGEN CONTAMINATION FROM THE CRUCIBLE IN BATCH-TYPE VACUUM INDUCTION MELTING[J]. Acta Metall Sin, 1965, 8(3): 392-394.
[1] 吴超万、李伟立、邵象华:金属学报,1964. 7、 145. [2] Electric Furnace Steelmaking, ed. C. E. Sims, (Interscience, 1963) , vol. 2, p. 136. [3] Wriedt, H. A., Chipman, J.: Trans. AIME 1956, 206, 1198. [4] Elliott, J. F., Gleiser, M.: Thermochemistry for Steelmaking, (Addison-Wesley, 1960) , vol. 1, p. 190.@ |
|