| 真空熔炼的物理化学 |
| 邵象华 |
| 冶金工业部钢铁研究院 |
|
| PHYSICAL CHEMISTRY OF VACUUM MELTING |
| SHAO HSIANG-HUA(Iron and Steel Research Institute; The Ministry of Metallurgical Industry) |
引用本文:
邵象华. 真空熔炼的物理化学[J]. 金属学报, 1964, 7(1): 85-103.
.
PHYSICAL CHEMISTRY OF VACUUM MELTING[J]. Acta Metall Sin, 1964, 7(1): 85-103.
[1] Werner, K.: Neue Hutte, 1962, (3) , 152. [2] Busch, J., Dodd, R. A.: Trans. AIME, 1960, 218, 488. [3] Kashyap, V. C., Parlee, N.: Trans. AIME, 1958, 212, 86. [4] Wagner, C.: Thermodynamics of Alloys, (Addison-Wesley, 1952) , p. 51. [5] Schenck, H., Frohberg, M. G., Graf, H.: Arch. Eisenhuttenw., 1958, 673. [6] Humbert, J. C., Elliott, J. F.: Trans. AIME, 1960, 218, 1076. [7] Pehlke, R. D., Elliott, J. F.: Trans. AIME, 1960, 218, 1088. [8] Turkdogan, E. T., Ignatowicz, S.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 1, p. 630. [9] Ohtani, M., Gokcen, N. A.: Trans. AIME, 1960, 218, 533. [10] #12 [11] Langenberg, F. C.: Trans. AIME., 1956, 206, 1024. [12] #12 [13] Fischer, W. A., Hoffmann, A.: Arch. Eisenhuttenw., 1960, 215. [14] Mund, A.: Stahl Eisen, 1962, 1485. [15] #12 [16] Smith, H. R. Jr.: Vacuum Metallurgy, ed. R. F. Bunshah, (Reinhold, 1958) , p. 228. [17] Fischer, W. A.: Arch. Eisenhuttenw., 1960, 1. [18] Olette, M.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 2, p. 1065. [19] Elliott, J. F., Gleiser, M.: Thermochemistry for Steelmaking, (Addison-Wesley, 1960) , vol. 1, p. 270-271. [20] Bockris, J. O'M., White, J. L., Mackenzie, J. D.: Physico-Chemical Measurements at High Temperatures, (Butterworths, 1959) , p. 369. [21] Fischer, W. A., Hoffmann, A.: Arch. Eisenhuttenw., 1960, 411. [22] Schenck, H., Domalski, H.-H.: Arch. Eisenhuttenw., 1961, 753. [23] Gill, G. M., Inerson, E., Austin, G. W.: J. Iron Steel Inst. (London). 1959, 191, 172. [24] 川畑正夫、橫田孝三、佐滕洋太、渡辺哲弥:铁钢,1960,46,1423. [25] 韓耀文:金属学报,1963,6,98. [26] 大野秢一:日本金属学会志,1959,23,489;493. [27] #12 [28] Fischer, W. A., Engelbrecht, H.: Stahl Eisen, 1955, 70. [29] Brotzmann, K.: Arch. Eisenhuttenw., 1960, 67. [30] Koros, P. J., Chipman, J.: Trans. AIME, 1956, 206, 1102. [31] Floridis, T. P., Chipman, J.: Trans. AIME, 1958, 212, 549. [32] Chipman, J.: J. Iron Steel Inst. (London), 1955, 180, 97. [33] 邹元爔:金属学报,1958,3,238. [34] #12 [35] 万谷志郞、的场幸雄:铁钢,1962,48,399. [36] Shiro Ban-ya, Sachio Matoba: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 1, p. 373. [37] #12 [38] #12 [39] Fuwa, T., Chipman, J.: Trans. AIME, 1959, 215, 708. [40] 八木貞之助、小野阳一:鉄鋼,1962,48,402. [41] 川畑正夫、渡辺哲弥:铁钢,1961,47,715. [42] #12 [43] 吳超万、李伟立、邵象华:待发表. [44] Wriedt, H. A., Chipman, J.: Trans. AIME, 1955, 203, 477. [45] #12 [46] Askoy, A. M.: Vacuum Metallurgy, ed. R. F. Bunshah, (Reinhold, 1958) , p. 65. [47] #12 [48] #12 [49] #12 [50] Chipman, J.: Basic Open Hearth Steelmaking, 2nd. ed., (AIME, 1951) , p. 676. [51] Bogdandy, L. V., Schmolke, R., Winzer, G.: Arch. Eisenhuttenw. 1958, 231. [52] Moore, J. H.: Metal Progr., 1953, 64, (10) , 105. [53] Wagner, C.: The Physical Chemistry of Steelmaking, ed. J. F. Elliott, (Wiley 1958) , p. 238. [54] King, T. B.: Vacuum Metallurgy, ed. R. F. Bunshah, (Reinhold, 1958) , p. 55. [55] Davey, T. R. A.: Trans. AIME, 1953, 197, 991. [56] #12 [57] Bogdandy, L. V., Dick, W., Stranski, I. N.: Arch. Eisenhuttenw., 1958, 329. [58] #12 [59] Darmara, F. N., Huntington, J. S., Machlin, E. S.: J. Iron Steel Inst. (London) 1959, 191, 266. [60] Parlee, N. A., Seagle, S. R., Schuhmann, R. Jr.: Trans. AIME, 1958, 212, 132. [61] Yang, L. (杨琳), Derge, G.: Physical Chemistry of Process Metallurgy, ed. G. R. St. Pierre, (Interscience, 1961) , pt. 1, p. 503. [62] Machlin, E. S.: Trans. AIME, 1960, 218, 314. [63] Bennett, G. H. J., Protheroe, H. T., Ward, R. G.: J. Iron Steel Inst. (London), 1960, 195, 174. [64] Hadley, R. L., Bianchi, L. M.: Vacuum Metallurgy, ed. J. M. Blocher, Jr., (Electrochemical Society Inc,, 1955) , p. 106. [65] #12 [66] #12 [67] 坂尾 弘,佐野幸吉:日本金属学会志,1962,26,30. [68] 坂尾 弘,佐野幸吉:日本金属学会志,1962,26,236;240. [69] Rist, A., Chipman, J.: Rev. Met. (Paris), 1956, 10, 796. [70] Chipman, J.: Trans. AIME, 1960, 218, 767. [71] Knuppel, H., Oeters, F.: Arch. Eisenhuttenw., 1962, 729. [72] Naeser, G., Scholz, W.: Stahl Eisen, 1959, 137. [73] d'Entremont, J. C., Guernsey, D. L., Chipman, J.: Trans. AIME, 1963, 227, 17. [74] Weinstein, M., Elliott, J. F.: Trans. AIME, 1963, 227, 285. [75] Ward, R. G.: J. Iron Steel Inst. (London), 1963, 201, 11. [76] Richardson, F. D., Dennis, W. E.: Trans. Faraday Soc., 1953, 49, 171. [77] Turkdogan, E. T., Leake, L. E., Masson, C. R.: Acta Met., 1956, 4, 396. [78] #12 [79] #12 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|