| 关于冷拔钢线低温退火后的二类畸变 |
| 胡玉和;杨春荣 |
| 鞍山钢铁公司;鞍山钢铁公司 |
|
| DETERMINATION OF MICROSTRESSES IN COLD-DRAWN WIRES AFTER LOW TEMPERATURE ANNEALING |
| HU YU-HUO;YANG CHUNG-YUNG Anshan Iron and Steel Corporation |
引用本文:
胡玉和;杨春荣. 关于冷拔钢线低温退火后的二类畸变[J]. 金属学报, 1963, 6(1): 74-82.
,
.
DETERMINATION OF MICROSTRESSES IN COLD-DRAWN WIRES AFTER LOW TEMPERATURE ANNEALING[J]. Acta Metall Sin, 1963, 6(1): 74-82.
[1] #12 [2] #12 [3] #12 [4] #12 [5] #12 [6] #12 [7] #12 [8] Andrew,J.H.,Lee,H.(李薰),Brookes,P.E.:J.Iron Steel Inst.,1950,165,369-374. [9] #12 [10] Greenough,G.B.:Progress in Metal Physics,(Butterworths,1952) ,vol.3,p.200-210. [11] Warren,B.E.:Progress in Metal Physics,(Pergamon,1959) ,vol.8,p.147-202. [12] Stokes,A.R.:Proc.Phys.Soc.,1948,61,382-391. [13] 陈篪、胡玉和:鞍纲中央试验室报告“用傅立叶级数法计算冷加工硅铁合金的真正线形”,1957年. [14] Jones,F.W.:Proc.Roy.Soc.,1938,A166,16-43. [15] #12 [16] #12 [17] #12 [18] #12 [19] #12 [20] #12 [21] #12 |
|