| 关于用提高温度法缩短高温蠕变试验的时间 |
| 孔庆平;林保军;葛庭燧 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| ON THE METHOD OF ACCELERATING HIGH-TEMPERATURE CREEP TEST BY AN ELEVATION OF TEMPERATURE |
| Kung Ching-ping; Lin Pao-chun; K? T'ing-sui Institute of Metal Research; Academia Sinica |
引用本文:
孔庆平;林保军;葛庭燧. 关于用提高温度法缩短高温蠕变试验的时间[J]. 金属学报, 1960, 5(1): 48-64.
,
,
.
ON THE METHOD OF ACCELERATING HIGH-TEMPERATURE CREEP TEST BY AN ELEVATION OF TEMPERATURE[J]. Acta Metall Sin, 1960, 5(1): 48-64.
[1] #12 [2] Larson, F. R. and Miller, J.: Trans. ASME, 74, (1952) , 765. [3] Betteridge, W.: J. Inst. Met., 86(1957-58) , 232. [4] Orr, R. L., Sherby, O. D. and Dorn, J. E.: Trans. ASM, 46(1954) , 113. [5] Dorn, J. E. Symposium on Creep and Recovery, (ASM 1957) , p. 255; J. Mech.phys. Solids, 3(1958) , 85. [6] Betteridge W.: The Nimonic Alloys(1959) . [7] Glen,J.: Iron and Steel, 28(1955) , 242. [8] #12 |
|