| 碳衬高炉炉缸内传热的若干问题 |
| 万纾民 |
| 中国科学院化工冶金研究所 |
|
| SOME PROBLEMS OF THE HEAT FLOW THROUGH THE BLAST FURNACE HEARTH WITH CARBON LINING |
| WAN SHU-MING Institute of Chemical Metallurgy; Academia Sinica |
引用本文:
万纾民. 碳衬高炉炉缸内传热的若干问题[J]. 金属学报, 1959, 4(3): 206-216.
.
SOME PROBLEMS OF THE HEAT FLOW THROUGH THE BLAST FURNACE HEARTH WITH CARBON LINING[J]. Acta Metall Sin, 1959, 4(3): 206-216.
[1] J. H. Chester, G. D. Elliot & J. Mackanzie, J. Iron and Steel Inst., 167 (1951) , 273. [2] Owen R. Rice, Ij Iron nnd Steel Inst., 170 (1952) , 89. [3] П. Н. Локшин и Т. П. 2 (1956) , 107. [4] J. Iron and Steel Inst., 170 (1952) , 139. [5] E. J. Williams and E. J. Burton, J. Iron and Steel Inst., 197 (1955) , 17. [6] J. Dobry, Hutnicke Listv, 11 (5) , (1956) 307. [7] V. Paschkis and Taghi Mirsepassi, Iron and Steel Engineer, 33, No. 6 (1956) , 116. [8] T. R. Westbrook, B. F. & S. P., 41, No. 4 (1953) , 413. [9] V. Paschkis, Iron and Steel Engineer, 31, No. 2 (1954) , 53. [10] И. Г. Половленкоo, 10 (1955) , 891. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|