| 高炉炉底耐火衬料的厚度及导热性对炉底温度场的影响 |
| 万纾民 |
| 中国科学院化工冶金研究所 |
|
| THE EFFECT OF THE THICKNESS AND THE THERMAL CONDUCTIVITIES OF THE REFRACTORY LININGS IN THE BLAST FURNACE BOTTOM ON THE TEMPERATURE FIELD OF THE BOTTOM |
| WAN SHU-MING Institute of Chemical Metallurgy; Academia Sinica |
引用本文:
万纾民. 高炉炉底耐火衬料的厚度及导热性对炉底温度场的影响[J]. 金属学报, 1959, 4(3): 195-205.
.
THE EFFECT OF THE THICKNESS AND THE THERMAL CONDUCTIVITIES OF THE REFRACTORY LININGS IN THE BLAST FURNACE BOTTOM ON THE TEMPERATURE FIELD OF THE BOTTOM[J]. Acta Metall Sin, 1959, 4(3): 195-205.
[1] 万纾民,碳衬高炉炉底传热中的若干问题(待发表). [2] T. R. Westbrook. BF&SP, 41, No. 4 (1953) , 413. [3] E. J. Williams and E. J. Burton, J. Iron and Steel Inst., 197 (1955) , 17. [4] V. Paschkis, Iron and Steel Engineer, 31, No. 2 (1954) , 53. [5] Ian N. Sneddon, Fourier Ttansforms, chap. 3, 1951. [6] В. В. Юшкин著,万纾民译,钢铁译丛,3(1958) ,4. [7] V. Paschkis and Taghi Mirsepassi, Iron and Steel Engineer, Junc (1956) ,116.! |
|