| THE WORK HARDENING OF METALS IN INDUSTRIAL PROCESSES OF PLASTIC DEFORMATION |
| W.TRUSZKOWSKI |
| InstituteofMetals;PolishAcademyofSciences |
|
| THE WORK HARDENING OF METALS IN INDUSTRIAL PROCESSES OF PLASTIC DEFORMATION |
| W. TRUSZKOWSKI Institute of Metals; Polish Academy of Sciences |
引用本文:
W.TRUSZKOWSKI. THE WORK HARDENING OF METALS IN INDUSTRIAL PROCESSES OF PLASTIC DEFORMATION[J]. 金属学报, 1959, 4(2): 139-142.
.
THE WORK HARDENING OF METALS IN INDUSTRIAL PROCESSES OF PLASTIC DEFORMATION[J]. Acta Metall Sin, 1959, 4(2): 139-142.
|