| 合金钢中微量希土元素(镧、铈、镨、钕)的定量光谱分析 |
| 李诗(钅卓);王玉梅 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| SPECTROGRAPHIC ANALYSIS OF SMALL AMOUNT OF RARE EARTHS IN ALLOY STEEL |
| LI SHUH-CHO;WANG YU-ME Institute of Metal Research; Academia Sinica |
引用本文:
李诗(钅卓);王玉梅. 合金钢中微量希土元素(镧、铈、镨、钕)的定量光谱分析[J]. 金属学报, 1959, 4(1): 81-86.
,
.
SPECTROGRAPHIC ANALYSIS OF SMALL AMOUNT OF RARE EARTHS IN ALLOY STEEL[J]. Acta Metall Sin, 1959, 4(1): 81-86.
[1] E. W. Spitz, J. R. Simmler, B. D. Field, K. H. Roberts and S. M. Tuthill, Ana. Chem. 26, 304, 1954. [2] 沈联芳等,化学学报 1958. [3] А. Н. Зайдель и др. Вестник ЛГУ 22,18,1956. |
|