| 铝火花法测定钢铁中的硼 |
| 王鸿漳 |
| 中国科学院金属研究所 |
|
| DETERMINATION OF BORON IN STEEL AND IRON BY THE ALUMINUM SPARK METHOD |
| WANG HONG-JANG Institute of Metal Research; Anademia Sinica |
引用本文:
王鸿漳. 铝火花法测定钢铁中的硼[J]. 金属学报, 1959, 4(1): 75-80.
.
DETERMINATION OF BORON IN STEEL AND IRON BY THE ALUMINUM SPARK METHOD[J]. Acta Metall Sin, 1959, 4(1): 75-80.
[1] E. F. Runge, L. S. Brooks and F. R. Bryan., Anal chem, 27, 1543, (1955) . [2] Soichiro Musha., Science Repts. Research Insts., Tohoku Univ. Ser. A. 2, 437, (1950) . [3] 曹思启.,钢铁工厂实验室,8, 22,(1957) . [4] B. I. S. R. A., J. Iron Steel, Inst. 189, 227, (1958) . [5] 村木勇夫,日色和夫.,化学译报,4,407,(1958) . [6] Everett C. Cogbill and John H. Yoe., Anal Chem, 29, 1251, (1957) . [7] W. G. Kirchgessner and N. A. Finkelstein., Anal Chem, 25, 1024, (1953) . [8] Ralph H. Steinberg., Applied Spectroscopy, 7, 176, (1953) . [9] О. В. Фалькова., ДАН, 48, 189. (1945) . [10] Naoichi Ota., Japan. Analyst, 2, 205, (1953) . [11] Fred M., J. O. S. A. 37, 279, (1947) . [12] Norman H. Nachtrieb: Principles and Practice of Spectrochemical Analysis. 261~277, (1950) ." |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|