摘要: 对国产工业纯铁在冶轧和热炼后的显微组织和磁性初步进行了试验。所用材料的轧制和再结晶结构已试测过,并叙述于前两篇报告里。具有较高的磁导率值的试样呈现二次再结晶.试样的再结晶组织和磁性的关系于本篇中作了简单的讨论.
Abstract:The microstructure and the magnetic properties of cold reduced and annealed armco iron arestudied.The textures of the samples used in the experiments have been determined by the X-raypole figure and the magnetic torque methods as reported in the two earlier papers.The samples having higher magnetic permeabilities show a secondary recrystallization.Therelations between recrystallization and magnetic properties are briefly discussed.
收稿日期: 1958-03-18     

引用本文:

戴孔智. 工业纯铁的再结晶与磁性[J]. 金属学报, 1958, 3(3): 227-230.
. THE RECRYSTALLIZATION AND MAGNETIC PROPERTIES OF ARMCO IRON. Acta Metall Sin, 1958, 3(3): 227-230.

链接本文:

https://www.ams.org.cn/CN/      或      https://www.ams.org.cn/CN/Y1958/V3/I3/227

[1] Say,M.G.,Magnetic Alloys and Ferrites,(1956) .
[2] Pawlek,F.,Magnetische Werkstoffe,Berlin,(1952) ,S.118,120.
[3] Bozorth,R.M.,Ferromagnetism,(1951) .P.56.
[4] Messkin,B.C.,(?),11(1947) .
[5] 戴礼智,张信钰,物理学报,14,(1958) ,17.
[6] 戴礼智,王建纲,金属学报,3(1958) ,45.
[7] Guihaumé,R.,Comptes Rend.,258(1954) ,2085.G
No related articles found!