| 锰对矽脱氧能力的影响 |
| 杜挺;A.M.蕯马林 |
|
| ВЛИЯНИЕ МАРГАНЦА НА РАСКИСЛИТЕЛЬНУЮ СПОСОБНОСТЬ КРЕМНИЯ В ЖИДКОМ ЖЕЛЕЗЕ |
| Ду Тинь;А.М.Самарин |
引用本文:
杜挺;A.M.蕯马林. 锰对矽脱氧能力的影响[J]. 金属学报, 1958, 3(3): 210-226.
,
.
ВЛИЯНИЕ МАРГАНЦА НА РАСКИСЛИТЕЛЬНУЮ СПОСОБНОСТЬ КРЕМНИЯ В ЖИДКОМ ЖЕЛЕЗЕ[J]. Acta Metall Sin, 1958, 3(3): 210-226.
[1] #12 [2] Chipman,J.,Gero,J.B.,Winkler,T.B.,The manganese equilibrium under simple oxide slags.Trans.AIME,188,(1950) ,341. [3] K(o|¨)rber,F.,Oelsen W.,Uber die Beziehungen zwischen manganhaltigen Eisen und Schlacken,die fast nur aus Manganoxydul und Eisenoxydul bestehen.Mitt.K.-W.Inst.14(1932) 181. [4] Hilty,D.C.,Crafts,W.,Solubility of oxygen in liquid iron containing silicon and manganese.J.of Metals 2(1950) ;Trans.AIME,188(1950) ,425. [5] Sloman,H.A.,Evans,E.L.,Deoxidation by manganese.J.Iron & Steel Inst.,169(1951) ,145. [6] #12 [7] Evans,E.L.,Sloman,H.A.,Dcoxidation by silicon.J.Iron & Steel Inst.,172(1952) ,296-300. [8] Hilty,D.C.,Crafts,W.,The solubility of oxygen in liquid iron containing aluminium.J.of Metals,2,(1950) ;Trans.AIME,188(1950) ,414. [9] Wentrup,H.,Hieber,G.,Umsetzungen zwischen Aluminium und Sauerstoff in Eisenschmelzen.Arch.Eisenhüttenwes.13(1939) ,15. [10] Hilty,D.C.,Forgen,W.D.,Folkman,R.L.,Oxygen solubility and oxide phases in the Fe-Cr-O system.J.of Metals,7(1955) ;Trans.AIME,203,(1955) ,253. [11] Evans,E.L.,Sloman,H.A.,Dioxidation by titanium.J.Iron & Steel Inst.,174(1953) ,318-324. [12] Wentrup,H.,Hieber,G.(U|¨)ber das Gleichgewicht zwischen Sauerstoff und Titan in Eisenschmelzen.Arch.Eisenhüttenwes.,13,(1939) ,69. [13] K(o|¨)rber,F.,Oelsen,W.Die Grundlagen der Desoxydation mit Mangan und Silizium,Mitt.K.-W.Inst, für Eisenforschung,15(1933) ,271-309. [14] #12 [15] #12 [16] #12 [17] Gokcen,N.A.,Chipman,J.Silicon-oxygen equilibrium in liquid iron.J.Metals,2,(1952) ;Trans.AIME,174(1952) ,171. [18] Gokcen,N.A.,Chipman,J.Silicon-oxygen equilibrium in liquid iron-A revision.J.Metals,5,(1953) ;Trans.AIME,197(1953) ,1017-1018. [19] Gokcen,N.A.,Chipman,J.Aluminum-oxygen equi(?)ibrium is liquid iron.J.Mctals,5,(1953) ;Trans.AIME 197(1953) ,173-178. [20] #12 [21] Pearson,J.,Turkdogan.E.T.Activity coefficients of oxygen and phosphorus in iron-oxygen-phosphorus melts.J.Iron & Steel Inst.,176,(1954) ,19-23. [22] #12 [23] Hsin-Min Chen,Chipman,J.The chromium-oxygen cquilibrium in liquid iron.Trans.ASM.38,(1947) ,70. [24] #12 [25] Basic open hearth process.New York,1951. [26] #12 [27] Marshall,S.,Chipman,J.The carbon-oxygen equilibrium in liquid iron.Trans.ASM,30,(1942) ,695. [28] #12 [29] #12 [30] #12 [31] #12 [32] #12 [33] #12 [34] #12 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|