| 制造金相样品胶质代替膜的“滴液盖片法” |
| 余仲奎;黃寿洪 |
| 华南工学院机械系;华南工学院机械系 |
|
| A PROCESS OF PREPARING REPLICAS FOR THE SUBSTITUTION OF METAL SPECIMENS IN METALLOGRAPHIC STUDY |
| C.F.YEE AND S.H.HUANG Engineering Institute of Southern China |
引用本文:
余仲奎;黃寿洪. 制造金相样品胶质代替膜的“滴液盖片法”[J]. 金属学报, 1958, 3(1): 80-84.
,
.
A PROCESS OF PREPARING REPLICAS FOR THE SUBSTITUTION OF METAL SPECIMENS IN METALLOGRAPHIC STUDY[J]. Acta Metall Sin, 1958, 3(1): 80-84.
[1] 阿雷克塞耶夫与赖赫西达脱合著,金属学分析方法、实验工作与习题,87页,重工业出版社,1954. [2] 马斯列尼科夫著,金属学实验,7页,1954. [3] Kehl,Principles of Metallographic Laboratory Practice(1949) ,3 ed.,148-150. [4] Journal of Applied Physics,14(1943) ,23-29. [5] Metal Progress,66(1954) ,No.1-A,175-177. [6] Metal Progress,67(1955) ,No.4,178. [7] Metal Treatment and Drop Forging,21(1954) ,103. [8] 余仲奎等,华南工学院学报第一期,1957年,金相标本胶质代替膜的研究与代替膜今后发展的方向. |
|