| 硼对珠光体成核及成长的影响 |
| 李林;祁明维;郑庆祺;苗永智 |
| 中国科学院冶金陶瓷研究所;中国科学院冶金陶瓷研究所;南京大学物理系;南京大学物理系 |
|
| THE EFFECT OF BORON ON THE NUCLEATION AND GROWTH OF PEARLITE |
| LEE LING;CHI MIN-WEI;CHUNG CHING-CHI;MEO YONG-TZE Institute of Metallurgy and Ceramics; Academia Sinica Nanking Unioersity; Department of Pkysics |
引用本文:
李林;祁明维;郑庆祺;苗永智. 硼对珠光体成核及成长的影响[J]. 金属学报, 1957, 2(1): 65-74.
,
,
,
.
THE EFFECT OF BORON ON THE NUCLEATION AND GROWTH OF PEARLITE[J]. Acta Metall Sin, 1957, 2(1): 65-74.
[1] Fisher, J. C., Influence of Boron on Hardenability of Steels, AIME, 1954, Vol. 200, p. 1146. [2] Wray, P. R., The Role of Boron Steels in the Present Emergency, Material and Methods, Aug., 1951. [3] Atlas of Isothermal Transformation Diagrams, 1951. [4] 李林,祁明维,硼-钼合金结构钢的研究,金属学报,第一卷,第三期,1956. [5] CCCP. [6] Spretnak, J. W. and Speiser, R., A Hypothesis for the Boron Hardenability Mechanism, ASM, 1954, Vol. 46, p. 1089. [7] Johnson, W. A. and Mehl, R. F., Reaction Kinetics in Process of Nucleation and Growth, AIME, 1939, Vol. 135, p. 416. [8] Simcoe, C. R., Elsea, A. R and Manning, G. K., Study of the Effect of Boron on the Decomposition of austenite, J. Metals, 1955, Jan., p. 193. [9] Rahrer, G. D. and Armstrong, C. D., The Effect of Carbon on the Hardenability of Boron Steels, A. S. M., 1948, Vol. 40, p. 1099. [10] Hull, F. C., Colton, R. A. and Mehl, R. F., Rate of Nucleation and Rate of Growth of Pearlite, AIME, 1942, Vol. 150, p. 185. [11] 1952, p. 260. [12] Zener, C., Kinetics of the Decomposition of austenite, Metals Technology, 1946, Jan. [13] 1955, p. 624. [14] Wells, C., Batz, W. and Mehl, R. F., Diffusion Coefficient of Carbon in austenite, AIME, 1950, Vol. 194, p. 533. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|