| NaCl和SO2在A3钢初期大气腐蚀中的协同效应 |
| 屈庆 严川伟 张蕾 万晔 曹楚南 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳110016 |
|
引用本文:
屈庆; 严川伟; 张蕾; 万晔; 曹楚南 . NaCl和SO2在A3钢初期大气腐蚀中的协同效应[J]. 金属学报, 2002, 38(10): 1062-1066 .
[1] Wang G Y, Wang H J, Li X L, Yin Y D. Corrosion and Protection in Natural Environment, Beijing: Chemical Industry Press, 1997: 1(王光雍,王海江,李兴濂,银耀德.自然环境的腐蚀与防护,北京:化学工业出版社,1997:1) [2] Wang Z Y. Master Thesis, Institute of Corrosion and Protection of Metals, The Chinese Academy of Sciences, Shenyang, 1994: 12(王振尧.中国科学院金属腐蚀与防护研究所硕士学位论文,沈阳,1994:12) [3] Wang Z Y, Zheng Y P, Yu G C, Li W Q. Corrosion Science and Protection Technology, 1999; 11: 306(王振尧,郑逸平,于国才,李文清.腐蚀科学与与防护技术,1999;11:306) [4] Kontkova D, Barton K, Tu B V. ASTM STP 965, edsDean S W, Lee T S. 1988: 290 [5] Lyon S B. Corrosion, 1987; 43: 719 [6] Svensson J E, Johansson L G. Corr Sci, 1993; 34: 721 [7] Qu Q, Yan C W, Bai W, Cao C N. Acta Metall Sin, 2001;37: 72(屈 庆,严川伟,白 玮,曹楚南.金属学报,2001;37:72) [8] Svensson J E, Johansson L G. Process 11th ScandinavianCorrosion Congress, Norway, Stavanger, 1989: F-47 [9] Qu Q, Yan C W, Wan Y, Cao C N. Corrosion Science,2002, to be published [10] Qu Q, Yan C W, Zhang L, CAO C N. J Mater Sci Technol. 2002, to be published [11] Wu J G. Techniques and Applications of Infrared Fourier Transform Spectroscopy, 2nd Volume. Beijing: Science and Technology Information Press, 1994: 269(吴瑾光.近代傅立叶变换红外光谱技术及应用.下卷,北京:科学技术文献出版社,1994:269) [12] Raman A, Kuban B, Razvan A. Corros Sci, 1991; 32: 1295 [13] Qu Q, Yan C W, Zhang L, Wan Y, Cao C N. Acta MetallSin (English Letter), 2002, to be published [14] Dawson J L, Ferreira M G. Corro Sci, 1986; 26: 1009 [15] Thomson G E, Johnson J B. Corrosion, 1987; 43: 719 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|